Chromium oxide (Cr2O5) → Bismuth oxide antimony oxide chromium oxide

HRID 1599352
Print

Reaction equation

HRID 1599352 reaction equation
[Bi:1]=[O:2].[Sb:3]=[O:4].[O-2].[Cr+3:6].[O-2].[O-2].[Cr+3]>>[Bi:1]=[O:2].[Sb:3]=[O:4].[O-2:2].[Cr+3:6].[O-2:2].[O-2:2].[Cr+3:6]
ParticipantsProcedureWorkupSources & evidenceReaction notes

Participants

4

Reactant 3

HCID 165971Chromium oxide (Cr2O5)HCID 6327673StibanalHCID 6327914Bismuth-oxygen2×

Product 1

HCID 131720612Bismuth oxide antimony oxide chromium oxide

Procedure

A bismuth oxide powder (whose average particle size is about 2 to 3 μm) and an antimony oxide powder (whose average particle size is about 2 to 3 μm) were blended at a weight ratio of 85:15. The blended powder was heat treated at a temperature of 550° C. for 5 hrs. in the air. Further, bismuth oxide fine particles (whose average particle size is about 2 to 3 μm) and chromium oxide fine powder (whose average particle size is about 0.5 to 1.5 μm) were mixed at a weight ratio of 75:25. The mixed powder was heat treated at a temperature of 550° C. for 5 hrs. in the air. These were blended at a weight ratio of 10:1 and ground fine for 18 hrs. by a wet method by means of stabilizing zirconia balls in a monomalon pot. Consequently, a synthetic powder of bismuth oxide/antimony oxide/chromium oxide (whose average particle size is about 2 to 3 μm) was obtained.

Workup

  1. temperatureThe blended powder was heat
  2. additiontreated at a temperature of 550° C. for 5 hrs
  3. temperatureThe mixed powder was heat
  4. additiontreated at a temperature of 550° C. for 5 hrs

Sources & evidence

ORD record
ord-cb3cde3623264b848480cf0eb89211d1
Source dataset
uspto-grants-1998_04
DOI
10.6084/m9.figshare.5104873.v1
Patent number
US05739742

Reaction notes