[C:1]([O:5]CCCCCC(C)C)(=[O:4])[CH:2]=[CH2:3].[C:14]([OH:18])(=[O:17])[CH:15]=[CH2:16]>C(OCC)(=O)C.CCCCCCC.CO>[C:1]([O-:5])(=[O:4])[CH:2]=[CH2:3].[C:14]([OH:18])(=[O:17])[CH:15]=[CH2:16]Isooctyl acrylate/acrylic acid (191.6 g, in a weight ratio of 98/2) pressure sensitive adhesive, as a 27 weight percent solution in ethyl acetate/heptane (2/3 weight ratio), was mixed with a 1.0 weight percent TTC as a solution in methanol (5.1 ml, AMRESCO, Solon, Ohio). This adhesive solution was initially colorless.