Reaction equation
P([O-])([O-])([O-])=O.[Al+3:6].[CH2:7](OP([O-])([O-])=O)[CH3:8].[OH2:14].CO[CH:17](O)[CH3:18]>>[CH3:17][CH2:18][CH:7]([O-:14])[CH3:8].[CH3:17][CH2:18][CH:7]([O-:14])[CH3:8].[CH3:17][CH2:18][CH:7]([O-:14])[CH3:8].[Al+3:6]Participants
Conditions
- Temperature
- 120 °C
Procedure
Comparative Example 1 involves the preparation of aluminum phosphate without using an organosilane. A homogeneous solution of aluminum s-butoxide (0.082 gm, 0.33 mmol) in methoxyethanol (0.5 ml) is prepared in a glass vial containing a magnetic stir bar. It is stirred for ½ hr after addition of ethylphosphate (0.06 gm, 0.33 mmol). Addition of DI water (0.010 gm, 0.56 mmol) results in the formation of a milky gel. After diluting with 0.5 ml methoxyethanol, the resulting milky solution is stirred at room temperature/overnight. Addition of DI water (0.010 gm, 0.56 mmol) followed by stirring at RT/overnight and 100° C./2 hrs generates white precipitates. The solution is applied to a glass plate to form a highly opaque non-uniform coating. White solid residues obtained after removing the volatiles are not soluble in methoxyethanol even heated to 120° C. in the presence of phenyltrimethoxysilane.
Workup
- additioncontaining a magnetic stir bar
- customresults in the formation of a milky gel
- stirringthe resulting milky solution is stirred at room temperature/overnight
- stirringby stirring at RT/overnight and 100° C./2 hrs
- customto form a highly opaque non-uniform coating
- customWhite solid residues obtained
- customafter removing the volatiles