Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Ethylene carbonate | HCID 7303 | — |
| Reactant | 2-(2-Hydroxypropoxy)-1-propanol | HCID 32881 | — |
| Catalyst | Sodium Stannate | HCID 21977542 | — |
| Product | Carbon Dioxide | HCID 280 | 14.7% |
| Product | Ethylene carbonate | HCID 7303 | 100% |
Reaction Steps
A 10:1 mole ratio of ethylene carbonate to dipropylene glycol is heated with stirring under a nitrogen atmosphere for 4 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 100 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 14.7 percent carbon dioxide The catalyst is removed as in Example 1.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04709069 |
|---|
| Source dataset | uspto-grants-1987_11 |
|---|
| ORD ID | ord-02a49089b68b4c768b9d92d5910ce35c |
|---|
| Source note | uspto-grants-1987_11 |
|---|