1,2-Diethenylbenzene → Styrene

HRID 351466

Reaction equation

HRID 351466 reaction equation
[CH:1]([C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][C:4]=1[CH:9]=[CH2:10])=[CH2:2].[Li]>>[CH2:2]=[CH:1][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH:1]([C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][C:4]=1[CH:9]=[CH2:10])=[CH2:2]

Participants

5

Procedure

A 10 μm-thick nonwoven fabric made of polyethylene (PE) was prepared. Then, divinylbenzene and lithium (Li) styrenesulfonate were impregnated in the fabric and then heated for thermal polymerization, resulting in formation of a thin-film of 10 μm thick with a copolymer of sulfonyl group-owning styrene and divinylbenzene being impregnated in the nonwoven fabric. This was cut into a portion having the cell size, which was then put on the EC layer.

Workup

  1. customwas prepared
  2. temperatureheated for thermal polymerization

Sources & evidence