Reaction equation
[CH2:1]=[CH:2][CH:3]=[CH2:4].[C:5]([O:9][CH2:10][CH2:11][O:12][CH3:13])(=[O:8])[CH:6]=[CH2:7]>>[CH2:1]=[CH:2][CH:3]=[CH2:4].[C:5]([O:9][CH2:10][CH2:11][O:12][CH3:13])(=[O:8])[CH:6]=[CH2:7]Participants
3
Procedure
A butadiene/2-methoxyethyl acrylate copolymer was synthesized as per Example 6, starting with 40 parts of butadiene and 60 parts of 2-methyoxyethyl acrylate. The isolated rubber exhibited a glass transition temperature of -60° C. and a Mooney viscosity of 37 (ML[4,100° C.]).