Reaction Steps

A solution of 8.6 g of capric acid in 100 ml of butyl acetate was maintained at a temperature of 5° C., to which 200 ml of water was added with stirring to form an emulsion. 50 ml of an aqueous solution of silver ammonium complex containing 8.5 g of silver nitrate (chillset at 5° C.) was added to the above emulsion over a 30 second period in order to allow the capric acid to react with the silver ion. After the removal of an aqueous phase, a silver caprate-containing butyl acetate phase was dispersed into 120 g of isopropanol solution containing 15 weight percent of polyvinyl butyral to produce a polymer dispersion of silver caprate. A composition containing the several components setforth below were added to the polymer dispersion of silver caprate in their listed order every ten minutes while maintaining the temperature at 50° C., resulting in the formation of a heat developable light-sensitive coating composition.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04128428
Source datasetuspto-grants-1978_12
ORD IDord-81fc92e20b984f1b88a2acdd24f8f212
Source noteuspto-grants-1978_12