HuagongsheHuagongshe Chemistry Print Report · For research reference only
endo-Dicyclopentadiene → Dicyclopentadiene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | endo-Dicyclopentadiene | HCID 15618652 | — |
| Catalyst | HCID 178479819 | HCID 178479819 | — |
| Product | Dicyclopentadiene | HCID 6492 | — |
Reaction Steps
Grubbs catalyst containing MCs (approximately 1 mg) were dispersed in neat DCPD (100 mg). The MCs were ruptured with a laser or by physical crushing. After rupturing, a gel was produced in approximately 10-30 minutes, with formation of a rubbery state, and then a solid resin over time. No gelling of DCPD was evident over two weeks with uncrushed MCs; however, the latent catalyst remained active as subsequent rupture of the MCs that had been left for five days still produced a gel in approximately 45-60 minutes. A background gelling rate of approximately 1 day was obtained with prepared particles that were not free flowing.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08822618B2 |
| Source dataset | uspto-grants-2014_09 |
| ORD ID | ord-28128eb9393442438c449ae2b9ebcc04 |
| Source note | uspto-grants-2014_09 |