Terephthalic Acid → Bis(2-hydroxyethyl) terephthalate

HRID 864275
Print

Reaction equation

HRID 864275 reaction equation
[C:1]([OH:12])(=[O:11])[C:2]1[CH:10]=[CH:9][C:5]([C:6]([OH:8])=[O:7])=[CH:4][CH:3]=1>C(O)CO>[C:1]([O:12][CH2:2][CH2:1][OH:11])(=[O:11])[C:2]1[CH:10]=[CH:9][C:5]([C:6]([O:8][CH2:5][CH2:6][OH:7])=[O:7])=[CH:4][CH:3]=1
ParticipantsProcedureSources & evidenceReaction notes

Participants

3

Reactant 1

HCID 7489Terephthalic Acid

Product 1

HCID 13739Bis(2-hydroxyethyl) terephthalate

Reagents, catalysts & solvents 1

HCID 174Ethylene GlycolSolvent

Procedure

Terephthalic acid was reacted with ethylene glycol to form bis-(2-hydroxyethyl) terephthalate and low oligomers thereof, in a standard direct esterification reaction. At the end of the direct esterification reaction 400 ppm of phosphoric acid stabiliser was added, followed by 500 ppm of antimony trioxide polycondensation catalyst and 500 ppm of "Irganox 1010" antioxidant. 0.3% of silica of particle size 4 μm, and 0.3% of titanium dioxide of particle size 0.2 μm were also added at this stage. A standard batch polycondensation reaction was performed until the intrinsic viscosity of the resultant polyethylene terephthalate was approximately 0.52. The polyethylene terephthalate was further polymerised by means of a batch solid phase polymerisation process, until the intrinsic viscosity (IV) of the polyethylene terephthalate was approximately 0.7 to 0.75. The solid phase polymerisation process utilised a fluidised bed, fluidised with nitrogen.

Sources & evidence

ORD record
ord-a2f9a7b3f9b94e5eb5167e5bd5f93d65
Source dataset
uspto-grants-1996_10
DOI
10.6084/m9.figshare.5104873.v1
Patent number
US05562984

Reaction notes

On this pageParticipantsProcedureSources & evidenceReaction notes