[CH3:1][C:2]([C:4]([NH:6][CH2:7][CH2:8][CH2:9][N+:10]([CH3:13])([CH3:12])[CH3:11])=[O:5])=[CH2:3].[Cl-:14].O.[CH:16]([OH:19])([CH3:18])C>>[CH3:3][C:2]([C:4]([NH:6][CH2:7][CH2:8][CH2:9][N+:10]([CH3:13])([CH3:11])[CH3:12])=[O:5])=[CH2:1].[Cl-:14].[CH:4]([N:6]1[CH2:7][CH2:8][CH2:18][C:16]1=[O:19])=[CH2:2]

Participants

4

Procedure

A polyethylene terephthalate (PET) surface is coated with an 8% solids solution of MAPTAC/VP/SiAM 15/75/10 of Example 1a (1.5 mL of solution on a 5 cm*5 cm PET sheet, spin coating 1500 rpm, 15 s). The solvent used is a water/isopropyl alcohol mixture (70/30), in order to have a sufficient wetting of the PET sheet by the solution. After 7 days of drying in 75% RH atmosphere, a contact angle of 140° is measured with water.

Workup

  1. customAfter 7 days of drying in 75% RH atmosphere
  2. customa contact angle of 140°