HomeMCPWorkbenchSkills
HomeWorkbenchNotificationsMe
llms.txt · MCP GuidePrivacy Policy · Terms of Service · Supportv1.8.3
  1. Home
  2. /Reaction

Palladium(II) nitrate dihydrate → Palladium nitrate

HRID 925009
Print

Reaction equation

HRID 925009 reaction equation
O.O.[N+:3]([O-:6])([O-:5])=[O:4].[Pd+2:7].[N+:8]([O-:11])([O-:10])=[O:9]>O>[N+:3]([O-:6])([O-:5])=[O:4].[Pd+2:7].[N+:8]([O-:11])([O-:10])=[O:9]
ParticipantsProcedureWorkupSources & evidenceReaction notes

Participants

3

Reactant 1

HCID 44134881Palladium(II) nitrate dihydrate

Product 1

HCID 24932Palladium nitrate

Reagents, catalysts & solvents 1

HCID 962WaterSolvent

Procedure

The nano ZnO (as described above) is further treated for the preparation of a photocatalyst of the present invention. The method include mixing a pre-determined amount of palladium(II) nitrate dihydrate (Pd(NO3)2.2H2O) in deionized water 414 to form enough solution to cover the required amount of nano-ZnO powder and form palladium nitrate impregnated nano-ZnO 416. The palladium nitrate impregnated nano-ZnO was then dried at heating rate of 1° C./min from room temperature up to 100° C. 418 and then exposed to ammonia vapors for another 10 min 420. This step is performed to avoid melting of palladium nitrate before decomposition resulting in high dispersion of nano Pd particles on ZnO. The palladium nitrate impregnated nano-ZnO was then dried overnight in air at a temp of 110° C. 422. The dried palladium nitrate impregnated nano-ZnO was calcined at 500° C. for 3 hours at a heating rate of 1.5° C./min to obtain a Pd-nano ZnO photocatalyst 424 (FIG. 1).

Workup

  1. customto form enough solution

Sources & evidence

ORD record
ord-bc99e2ba9ee84379b2341d7afdc3fd86
Source dataset
uspto-grants-2016_03
DOI
10.6084/m9.figshare.5104873.v1
Patent number
US09283546B2

Reaction notes

On this pageParticipantsProcedureWorkupSources & evidenceReaction notes