Procedure
To this inhibited epoxy diester-styrene mixture 5.49 parts of NADIC methyl anhydride, 0.048 part of 2,5-dimethyl-2,5 bis(benzoyl peroxy) hexane catalyst (sold by Wallace & Tierman Inc. under the tradename of Luperox 118), and 0.05 part of zinc ethyl hexoate catalyst were added, at 25° C., to provide the solventless epoxy-styrene varnish. The viscosity of the epoxy-styrene resin was measured to be about 200 cps at 25° C.