戻る
化工社化工社 化学情報印刷レポート · 研究参考用
HRID 10115作成日:2026年10月25日

Ammonium Oxalate → Cerous oxalate

https://huagongshe.com/reaction/10115

反応式

関与物質

役割名称HCID仕込み量
反応物Ammonium OxalateHCID 14213—
反応物Cerium(III) chlorideHCID 24636—
反応物Cerium oxideHCID 9905479—
生成物Cerous oxalateHCID 165565—

反応条件

温度1500 °C

反応手順

A cerium oxalate powder was prepared by adding an aqueous solution of ammonium oxalate to an aqueous solution of cerium chloride under stirring, causing the precipitation of cerium oxalate, filtering, and drying. The powder was ground with a jet-mill to obtain a starting material powder with a mean particle diameter of about 1 μm. The powder was ejected at a feed rate of 5 kg/hr through a nozzle with a cross-sectional area of the opening of 0.13 cm2 together with air at a flow rate of 200 L/min as a carrier gas into a reaction tube heated to a temperature of 1500° C. in an electric furnace, passed through the reaction tube, while maintaining the dispersion concentration of the powder, and heated. The melting point of cerium oxide is about 1950° C. The dispersion concentration of the starting material powder in the gas phase inside the reaction tube was 0.4 g/L, and V/S was 1500. The light-yellow powder thus produced was collected with a bag filter.

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US07094289B2
出典データセットuspto-grants-2006_08
ORD IDord-c817a0ea0ac64877a846f4b006c3f5c4
出典メモuspto-grants-2006_08