戻る
化工社化工社 化学情報印刷レポート · 研究参考用
HRID 1033372作成日:2026年10月27日

Styrene → Acrylonitrile butadiene styrene

https://huagongshe.com/reaction/1033372

反応式

関与物質

役割名称HCID仕込み量
反応物StyreneHCID 7501—
反応物AcrylonitrileHCID 7855—
生成物Acrylonitrile butadiene styreneHCID 24756—

反応手順

The procedure of Example 1 was repeated except a total of 273 grams of acrylonitrile was used instead of the total of 546 grams as per Example 1. In this example, the incremental addition was repeated except only one half of each amount of acrylonitrile was used. A portion of the latex was isolated for subsequent blending and the remaining latex coagulated as per Example 1. The dry rubber had a Mooney viscosity (100° C.) of 127, a bound acrylonitrile content of 3.8 weight percent (by Carlo Erba nitrogen analysis), a bound styrene content of 40.4 weight percent (by FTIR analysis) and a glass transition temperature of -28° C. (by DSC, Differential Scanning Calorimetry).

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US05310815
出典データセットuspto-grants-1994_05
ORD IDord-7a76b736098d4b88bd55064f5ab5fd18
出典メモuspto-grants-1994_05