反応式
O.O.O.O.O.O.[N+:7]([O-:10])([O-:9])=[O:8].[Mg+2:11].[N+:12]([O-:15])([O-:14])=[O:13]>O>[N+:7]([O-:10])([O-:9])=[O:8].[Mg+2:11].[N+:12]([O-:15])([O-:14])=[O:13]参加物
3
実験手順
4.1 parts by weight of water and 1 part by weight of magnesium nitrate hexahydrate were mixed to provide a solution of magnesium nitrate. The thus prepared solution of aqueous magnesium nitrate was applied to a glassware article utilizing substantially identical conditions as those employed in Example 1. The resulting "hot end" coating was transparent and attractive in appearance, and the article after "cold end" coating provided good lubrication both dry and wet when tested in a manner identical to that utilized in Example 1.
出典と根拠
- ORDレコード
- ord-fe5e366636bc45f7ab738d8ffac95f94
- 出典データセット
- uspto-grants-1981_09
- 特許番号
- US04289816