反応式
C=CC1C=CC=CC=1.[C:9]([O:14]C)(=[O:13])[C:10]([CH3:12])=[CH2:11].[C:16](OCCCC)(=[O:19])C=C.C(N)(=[O:29])C(C)=C.C(OCCO)(=O)C=C.C(OC)(=O)C(C)=C.C(O)(=O)C(C)=C.N>O>[OH:19][CH2:16][CH2:12][C:10](=[CH2:11])[C:9]([O:14][OH:29])=[O:13]参加物
5
実験手順
This example illustrates a graft copolymer according to the present invention comprising 94% backbone made from styrene/methyl methacrylate/n-butyl acrylate/methacrylamide/2-hydroxyethyl acrylate (in the weight ratio of 27/14.5/46/4/2.5) and 6% macromonomer (from Example 1) made from methyl methacrylate/methacrylic acid (in the weight ratio of 3.6/2.4). This graft copolymer copolymerized after dispersion in water using ammonia to form a high molecular weight binder with both hydroxy (2-hydroxyethyl acrylate) and amide (methacrylamide) functionalities. The following components were used in the preparation:
出典と根拠
- ORDレコード
- ord-e621c2bd7cc14055a8c415b50f9f13ad
- 出典データセット
- uspto-grants-1999_08
- 特許番号
- US05936026
関連ノート