反応式
[OH:1][C:2]1[CH:9]=[CH:8][C:5]([CH:6]=[CH2:7])=[CH:4][CH:3]=1.[C:10]([O:14][C:15]1[CH:22]=[CH:21][C:18]([CH:19]=[CH2:20])=[CH:17][CH:16]=1)([CH3:13])([CH3:12])[CH3:11].C(OC=C)C>>[CH2:10]([O:14][C:15]1[CH:22]=[CH:21][C:18]([CH:19]=[CH2:20])=[CH:17][CH:16]=1)[CH3:11].[OH:1][C:2]1[CH:9]=[CH:8][C:5]([CH:6]=[CH2:7])=[CH:4][CH:3]=1.[C:10]([O:14][C:15]1[CH:16]=[CH:17][C:18]([CH:19]=[CH2:20])=[CH:21][CH:22]=1)([CH3:13])([CH3:11])[CH3:12]参加物
3
実験手順
Using 26.8 g of poly(p-hydroxystyrene/p-tert-butoxystyrene) obtained according to (2) above and 1.5 g of ethylvinyl ether, reaction and after-treatments were carried out according to (3) of Preparation Example 1 to obtain 25.0 g of poly(p-1-ethoxystyrene/p-hydroxystyrene/p-tert-butoxystyrene) as white powdery crystal. P-1-ethoxyethoxystyrene unit/p-hydroxystyrene unit/p-tert-butoxystyrene unit molar ratio in the polymer≈10:65:25. Mw≈1 9,200; Mw/Mn=1.30 (GPC with polystyrene calibration).
後処理
- customobtained
出典と根拠
- ORDレコード
- ord-c426c153e0234b839b8ab31a169f8f73
- 出典データセット
- uspto-grants-1999_11
- 特許番号
- US05976759
関連ノート
読み込み中…