化工社化工社 化学情報印刷レポート · 研究参考用
Sodium Tetradecyl Sulfate → Benzene, ethenyl-, polymer with 1,3-butadiene
関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|---|---|---|
| 反応物 | Sodium Tetradecyl Sulfate | HCID 23665772 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | Benzene, ethenyl-, polymer with 1,3-butadiene | HCID 62697 | — |
反応手順
The material was prepared by dispersing 0.80 g Tergitol TMN-06 in 1481 g deionized water with an air mixer. To this was then added 1159 g of ground crystalline silicotitanate (150 g, 13.0% solids) (IONSIV IE 910) with agitation. Slowly to this was added 150.1 g Goodrite 1800×73 (39% solids, 58.5 g) with stirring. This mixture was mixed for 1 hour with an air mixer. The slurry was spray dried using a Niro Atomizer, (Serial number #2402) at 35 mL/min. Spray drying conditions were as follows:
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 特許番号 | US05989434 |
| 出典データセット | uspto-grants-1999_11 |
| ORD ID | ord-e2d357fa244044eeb976b4fe3b6f5260 |
| 出典メモ | uspto-grants-1999_11 |