関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Phenol | HCID 996 | — |
| 反応物 | Aluminum | HCID 5359268 | — |
| 生成物 | Phenol, aluminum salt (3:1) | HCID 167236 | — |
反応手順
In a reaction vessel was placed 8100 parts of phenol and 27 parts of aluminum metal. The vessel was sealed and heated to 150° C. to form aluminum triphenoxide. This catalyst concentrate was then mixed with 11,124 parts of additional phenol. This gives a phenol/aluminum mole ratio of about 203. The phenol-catalyst mixture was cooled to 90° C. and 23,490 parts of isobutylene was pumped in over a 50-minute period. The reaction temperature rose to 110° during the first 10 minutes of isobutylene feed. Stirring was continued at 110°-115° C. for 165 minutes. Reactor pressure dropped to 120 psig from a maximum of 260 psig.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US04870215 |
|---|
| 出典データセット | uspto-grants-1989_09 |
|---|
| ORD ID | ord-8d821badf57d4ee381083a26d3e3255c |
|---|
| 出典メモ | uspto-grants-1989_09 |
|---|