関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | 2-Ethylhexanoic Acid | HCID 8697 | — |
| 反応物 | Bismuth | HCID 5359367 | — |
| 反応物 | Hexanoic acid, 2-ethyl-, ammonium salt | HCID 57370172 | — |
| 溶媒 | Methanol | HCID 887 | — |
| 生成物 | Bismuth tris(2-ethylhexanoate) | HCID 3034787 | — |
反応手順
The electrolyzer of FIG. 1 was used to assist the reaction. The anolyte contained a solution formed from 10 ml of 2-ethylhexanoic acid, 1.6 g of ammonium 2-ethylhexanoate, and 90 ml of methanol. The anode was a bismuth plate having a surface area of 10 cm2. The catholyte solution contained 3 ml of 2-ethylhexanoic acid, 0.5 g of ammonium 2-ethylhexanoate, and 27 ml of methanol. A graphite cathode having a surface area of 10 cm2 was utilized. Electrolysis was conducted using a current of 0.100 amps for 20 hours. A 2 ml quantity of 2-ethylhexanoic acid was added to the catholyte solution every 3 hours. The anolyte solution was removed from the electrolyzer and filtered. The mother liquor was cooled to a temperature ranging from about 0-2° C. to precipitate crystals. The crystals were isolated by filtration, washed with methyl alcohol, and dried in a vacuum heater at a temperature ranging from about 50-60° C. for a duration of 7-8 hours. The product included 14.3 g of a viscous transparent liquid, namely, Bi(C7H15COO)3. Table 2 presents the analytical data for the product.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US06033551 |
|---|
| 出典データセット | uspto-grants-2000_03 |
|---|
| ORD ID | ord-1e6d32919588491bbe8023e4b2c6d377 |
|---|
| 出典メモ | uspto-grants-2000_03 |
|---|