反応式
[C:1](S(O[Li])=O)([C:4](C(C(C([C:16]([C:19]([C:22]([F:25])([F:24])[F:23])(F)[F:20])([F:18])[F:17])(F)F)(F)F)(F)F)([F:6])[F:5])([F:3])[F:2]>O>[F:23][C:22]([F:25])([F:24])[C:19]([F:20])=[C:16]([F:18])[F:17].[F:2][C:1]([F:3])=[C:4]([F:6])[F:5]参加物
3
試薬・触媒・溶媒 1
実験手順
A 400 ml autoclave was loaded with 100 ml water and 1.0 g of C8F17SO2Li. The autoclave was cooled, evacuated, and loaded with 75 g of hexafluoropropylene and 50 g of tetrafluoroethylene. A solution of 0.5 g of sodium bromate in 50 ml of water was injected over about 3 to 4 hours at 20° to 25° C. The autoclave was vented, the polymeric emulsion recovered, and the emulsion broken by freezing. Filtering, washing 10 times with 200 ml of 1:1 methanol/water, and drying under vacuum gave 31 g of hexafluoropropylene/tetrafluoroethylene copolymer too high in molecular weight to extrude in a melt index apparatus at 372° C. with a 15 kg weight.
後処理
- temperatureThe autoclave was cooled
- customevacuated
- customthe polymeric emulsion recovered
- filtrationFiltering
- washwashing 10 times with 200 ml of 1:1 methanol/water
- customdrying under vacuum
出典と根拠
- ORDレコード
- ord-47c6e2116e3944939088f0a2ddf44b07
- 出典データセット
- uspto-grants-1997_06
- 特許番号
- US05639837
関連ノート
読み込み中…