戻る
化工社化工社 化学情報印刷レポート · 研究参考用
HRID 1758776作成日:2026年10月27日

Cyclohexyl methacrylate → divinylbenzene cyclohexyl methacrylate N,N-diethylaminoethyl methacrylate

https://huagongshe.com/reaction/1758776

反応式

関与物質

役割名称HCID仕込み量
反応物Cyclohexyl methacrylateHCID 7561—
反応物Stearyltrimethylammonium chlorideHCID 8155—
反応物Potassium PersulfateHCID 24412—
反応物1,2-DiethenylbenzeneHCID 66666—
反応物Sodium BisulfiteHCID 23665763—
溶媒WaterHCID 962—
生成物divinylbenzene cyclohexyl methacrylate N,N-diethylaminoethyl methacrylateHCID 70529907—

反応条件

温度60 °C

反応手順

216 g of distilled water was placed in a reaction vessel, deaerated with a nitrogen gas, and heated to 60° C. in the presence of the nitrogen gas. 15.8 g of stearyltrimethylammonium chloride, 0.07 g of polyvinyl alcohol, 33.7 g of cyclohexyl methacrylate, 37.1 g of N,N-diethylaminoethyl thacrylate, and 2.0 g of divinylbenzene were added thereto. Then, 0.44 g of potassium persulfate dissolved in 9.3 ml of distilled water deaerated with a nitrogen gas, and 0.14 g of sodium hydrogensulfite dissolved in 1.5 ml of distilled water deaerated with a nitrogen gas were simultaneously added thereto, and heated for about one hour. Subsequently, the above-described potassium persulfate aqueous solution and the sodium hydrogensulfite aqueous solution were again added thereto, followed by continuing heating for about 5 hours. Then, the system was cooled to room temperature, and filtered to obtain a polymer dispersion containing 22.8 wt% solids.

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US04374924
出典データセットuspto-grants-1983_02
ORD IDord-9ca22283ed3a4bdb91f2b44e8c000613
出典メモuspto-grants-1983_02