関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Propylene | HCID 8252 | — |
| 反応物 | Cyclohexane, (dimethoxymethylsilyl)- | HCID 569301 | — |
| 反応物 | Triethylaluminum | HCID 16682930 | — |
| 触媒 | Titanium | HCID 23963 | — |
| 生成物 | Decane | HCID 15600 | — |
反応手順
400 ml purified decane was introduced into a glass autoclave with an internal volume of 500 ml purged sufficiently with nitrogen, and the liquid phase and gaseous phase were saturated by blowing 100 liters/h propylene. Thereafter, 10 mmol triethyl aluminum, 1.0 mmol cyclohexyl methyl dimethoxy silane, and the solid titanium component (a) in an amount of 0.2 mmol in terms of titanium atom were added in this order. The mixture was polymerized at 100° C. for 2 hours while the flow rate of propylene was regulated such that the unreacted gas was not leaked out through a bubbler tube connected a purge line and the inside of the reactor was not under reduced pressure. Then, the propylene gas was replaced by a nitrogen gas with which the unreacted propylene gas was purged to terminate the reaction, to give decane slurry containing polypropylene modified at the terminal thereof.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US07067587B2 |
|---|
| 出典データセット | uspto-grants-2006_06 |
|---|
| ORD ID | ord-fd1ebadb748c481581d3257476822cee |
|---|
| 出典メモ | uspto-grants-2006_06 |
|---|