戻る
化工社化工社 化学情報印刷レポート · 研究参考用
HRID 1968370作成日:2026年10月26日

Phosphoric Acid → Yttrium oxide

https://huagongshe.com/reaction/1968370

反応式

関与物質

役割名称HCID仕込み量
反応物Phosphoric AcidHCID 1004—
反応物YttriumHCID 23993—
反応物Yttrium oxideHCID 159374—
生成物Yttrium oxideHCID 159374—
生成物Yttrium phosphateHCID 10313406—

反応手順

Generally, a 75 to 85 weight percent solution of phosphoric acid is added to the slurry over a period of about 15 minutes to about 90 minutes as the slurry is continuously agitated and maintained at a temperature that typically ranges between about 20° C. and about 70° C. The amount of the phosphoric acid added to the slurry is usually about 1.5 molar percent less than the amount of the yttrium compound present in the slurry. When the yttrium compound used is yttrium oxide, the reaction takes place to form yttrium phosphate, minor amounts of yttrium oxide, minor amounts of surface adsorbed phosphoric acid and water. The yttrium phosphate formed comprises approximately 95.5 percent of the solids portion in the slurry.

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US08425871B2
出典データセットuspto-grants-2013_04
ORD IDord-6133381c1d1f40118090b7162bf7793b
出典メモuspto-grants-2013_04