関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Methane | HCID 297 | — |
| 反応物 | Formaldehyde | HCID 712 | — |
| 反応物 | Resorcinol | HCID 5054 | — |
| 反応物 | Sodium Hydroxide | HCID 14798 | — |
| 反応物 | Ammonium Hydroxide | HCID 14923 | — |
| 反応物 | Dipentamethylenethiuram tetrasulfide | HCID 61049 | — |
| 反応物 | Magnesium monoxide | HCID 6850729 | — |
| 反応物 | 6-((3-fluoro-5-(1-methoxycyclohexyl)phenoxy)methyl)quinolin-2(1H)-one | HCID 14985873 | — |
| 触媒 | Nickel bis(dibutyldithiocarbamate) | HCID 6101499 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | 2,6-Dihydroxybenzaldehyde | HCID 10285801 | — |
反応手順
Resorcinol formaldehyde adhesive latexes (RFL) were prepared from the latex by mixing 40 parts of a 4.72% aqueous resorcinol solution, 2.77 parts of a 37% aqueous formaldehyde solution, and 36.5 parts of the 47% solids copolymer latex and 20 parts of 15% aqueous sodium hydroxide (catalyst); adjusted to 20.6% solids with water and brought to a pH of 9.9 by addition of a 28% aqueous ammonium hydroxide solution. Nylon 66 fabric was treated with the RFL and heat activated. The treated fabric was then passed between two slabs of chlorosulfonated polyethylene compounded with 10 phr (parts per hundred parts rubber) magnesium oxide, 20 phr litharge, 40 phr SRF carbon black, 2 phr dipentamethylenethiuram tetrasulfide, 0.25 phr bis-benzothiazonyl sulfide and 3 phr nickel dibutyldithiocarbamate. The rubber slabs were then cured for 30 minutes at 153° C. The force required to pull the rubber and fabric apart, determined according to ASTM D-2138, was 28 pli with 80% rubber tear.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US05234989 |
|---|
| 出典データセット | uspto-grants-1993_08 |
|---|
| ORD ID | ord-e6b84081f91b47c89339903fcc7bd3b5 |
|---|
| 出典メモ | uspto-grants-1993_08 |
|---|