関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Methanesulfonic Acid | HCID 6395 | — |
| 反応物 | Styrene | HCID 7501 | — |
| 反応物 | Trichlorosilane | HCID 24811 | — |
| 触媒 | Platinum | HCID 23939 | — |
| 溶媒 | Toluene | HCID 1140 | — |
| 生成物 | (2-Phenylethyl)trichlorosilane | HCID 70327 | 8.7% |
反応手順
Reaction between styrene and trichlorosilane with platinum catalyst in the presence of a trimethylsilyl ester of methanesulfonic acid. 518 mg Styrene and 694 mg trichlorosilane were introduced into a glass tube, and 42 mg of a trimethylsilyl ester of methanesulfonic acid were added. 2.5 mg Of a toluene solution of a 0-valent platinum complex of divinylsiloxane (0.04 wt % platinum content) were added. The tube was sealed with Teflon tape and a rubber septum and placed in a 50° C. oil bath where it was heated for 30 minutes. After cooling, the tube contents were analyzed by gas chromatography revealing a styrene conversion of 11% and a phenethyltrichlorosilane yield of 8.7%. The ratio between the phenethyltrichlorosilane and the (α-methylbenzyl)trichlorosilane was 390:1.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US06326506B1 |
|---|
| 出典データセット | uspto-grants-2001_12 |
|---|
| ORD ID | ord-fe3869d0f04b408885da9502edf12f1a |
|---|
| 出典メモ | uspto-grants-2001_12 |
|---|