反応式
O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.[S:19]([O-:23])([O-:22])(=[O:21])=[O:20].[Al+3:24].[S:25]([O-:29])([O-:28])(=[O:27])=[O:26].[S:30]([O-:34])([O-:33])(=[O:32])=[O:31].[Al+3]>O>[S:19]([O-:23])([O-:22])(=[O:21])=[O:20].[Al+3:24].[S:25]([O-:29])([O-:28])(=[O:27])=[O:26].[S:30]([O-:34])([O-:33])(=[O:32])=[O:31].[Al+3:24]参加物
3
実験手順
To the aqueous polymer mixture was added 1.0 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.
後処理
- additionThe polymer mixture was then mixed for 30 minutes
- customto provide a crosslinked polymer gel
出典と根拠
- ORDレコード
- ord-4099d1be7b444480aa6230029cba152d
- 出典データセット
- uspto-grants-2014_02
- 特許番号
- US08641869B2
関連ノート
読み込み中…