[CH3:1][C:2]1[CH:3]=[CH:4][C:5]([OH:24])=[C:6]([C@@H:8]([C:18]2[CH:19]=[CH:20][CH:21]=[CH:22][CH:23]=2)[CH2:9][CH2:10][N:11]([CH:15]([CH3:17])[CH3:16])[CH:12]([CH3:14])[CH3:13])[CH:7]=1.C(O)(C(O)=O)C(O)C(O)=O>O>[CH3:1][C:2]1[CH:3]=[CH:4][C:5]([OH:24])=[C:6]([C@@H:8]([C:18]2[CH:19]=[CH:20][CH:21]=[CH:22][CH:23]=2)[CH2:9][CH2:10][N:11]([CH:12]([CH3:14])[CH3:13])[CH:15]([CH3:16])[CH3:17])[CH:7]=1参加物
3
実験手順
Tolterodine tartrate, microcrystalline cellulose and part of ethylcellulose are blended with small amount of water into homogeneous blend from which pellet cores are made by extrusion and spheronization. Dry pellet cores are coated with the coating dispersion of Example 8. Within first hour almost 50% dissolves, however between 7 and 16 hours less dissolves as compared to Example 2.
後処理
- customDry pellet cores
- dissolutionWithin first hour almost 50% dissolves, however between 7 and 16 hours
- dissolutionless dissolves
出典と根拠
- ORDレコード
- ord-cc18d6845501455995a9f42bb0d6eea0
- 出典データセット
- uspto-grants-2014_02
- 特許番号
- US08642078B2
関連ノート
読み込み中…