関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Ethylene carbonate | HCID 7303 | — |
| 触媒 | Sodium metaborate | HCID 145326 | — |
| 溶媒 | Diethylene Glycol | HCID 8117 | — |
| 生成物 | Carbon Dioxide | HCID 280 | 17.8% |
| 生成物 | Ethylene carbonate | HCID 7303 | 100% |
反応手順
A 50:1 mole ratio of ethylene carbonate to diethylene glycol is heated with stirring under a nitrogen atmosphere for 45 hours at 160° C. using 1.0 percent sodium metaborate as catalyst to give 100 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 17.8 percent carbon dioxide. The catalyst is removed as in Example 1.