関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Formaldehyde | HCID 712 | — |
| 反応物 | Sulfuric Acid | HCID 1118 | — |
| 反応物 | Melamine | HCID 7955 | — |
| 反応物 | Metasilicic acid | HCID 14768 | — |
| 反応物 | Orthosilicic acid | HCID 14942 | — |
| 生成物 | Formaldehyde melamine silicate melamine | HCID 131710832 | — |
反応手順
The mixture of polysiliconformic acid, orthosilicoformic acid, silicoformic acid and metasilicic acid as produced in Example XIV are mixed with 30 parts by weight of melamine and added to 100 parts by weight of an aqueous solution containing about 37% formaldehyde, then dilute sulfuric acid is added until the pH is 4 to 6. The mixture is heated to 70° to 100° C., while agitating; the silicic acid and melamine go into solution, and, in 20 to 60 minutes or until the desired viscosity is obtained, produces a white poly (formaldehyde melamine silicate melamine silicoformate) resin. The said resin softens with heat and may be molded into useful objects. The said resin is soluble in acetic acid and, when applied to wood and dried, it produces a tough clear protective coating.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US04033935 |
|---|
| 出典データセット | uspto-grants-1977_07 |
|---|
| ORD ID | ord-cf9fd26add1b4205882bdf954c50550f |
|---|
| 出典メモ | uspto-grants-1977_07 |
|---|