関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Ethylene | HCID 6325 | — |
| 反応物 | Boron trifluoride | HCID 6356 | — |
| 反応物 | Azobisisobutyronitrile | HCID 6547 | — |
| 反応物 | Maleic Anhydride | HCID 7923 | — |
| 反応物 | Ethyl Acrylate | HCID 8821 | — |
| 反応物 | Allyl acrylate | HCID 13835 | — |
| 溶媒 | Acetone | HCID 180 | — |
| 溶媒 | Dichloromethane | HCID 6344 | — |
| 生成物 | Ethylene/Ethyl Acrylate Allyl Acrylate Maleic Anhydride | HCID 86737232 | — |
反応手順
A 7.57-liter stirred autoclave was charged under nitrogen with 4000 ml. of methylene chloride, 400 grams of ethyl acrylate, 20 grams of maleic anhydride, 1.2 grams of allyl acrylate, and 1.0 gram of azobis(isobutyronitrile). It was then sealed, charged with 300 grams of boron trifluoride, and pressured to 21 kg./sq. cm. with ethylene. The subsequent copolymerization at 25° C. was continued until pressure measurement indicated that ethylene uptake had ceased (about two hours later). The reaction was quenched by addition of one liter of diethyl ether. Volatiles were removed by steam-stripping in a well-ventilated hood. The terpolymer thereby obtained was dissolved in acetone, precipitated in water in a blender, and oven-dried. Yield: 415 grams.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US04225476 |
|---|
| 出典データセット | uspto-grants-1980_09 |
|---|
| ORD ID | ord-64a9bf2ab9ad4033bab0329dec4fa910 |
|---|
| 出典メモ | uspto-grants-1980_09 |
|---|