実験手順
thermally reacting titanium dioxide and phosphoric acid at a temperature of about 400° C. to about 500° C. in a reaction mixture having a phosphorus pentoxide to titanium dioxide mole ratio of about 1.20 to about 1.25 to form a fine titanium pyrophosphate powder with greater than 90% of said fine titanium pyrophosphate powder having a particle size less than 1 micron in diameter; and
後処理
- customat a temperature of about 400° C. to about 500° C.