関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Sulfuric Acid | HCID 1118 | — |
| 反応物 | Aluminum Hydroxide | HCID 10176082 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | Aluminum Sulfate | HCID 24850 | — |
反応手順
The process 300 begins with a reaction step 308 wherein the aluminum hydroxide is fed, either as a wet cake or as a dry powder, with a slurry water 310 and an acid 312 into a pressure cooker. The acid 312 can be sulfuric acid. The temperature is raised to approximately 150° C. to produce an aluminum sulfate in a molten hydrate form. The pressure is held high enough to maintain a liquid state, e.g., 1100 kilo-Pascals. The residence time is between one to ten minutes, and preferably about two minutes.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US06221233B1 |
|---|
| 出典データセット | uspto-grants-2001_04 |
|---|
| ORD ID | ord-45af5e9f1c8a46cea3e4e406db790031 |
|---|
| 出典メモ | uspto-grants-2001_04 |
|---|