戻る
化工社化工社 化学情報印刷レポート · 研究参考用
HRID 379496作成日:2026年10月27日

Lactide → Poliglecaprone

https://huagongshe.com/reaction/379496

反応式

関与物質

役割名称HCID仕込み量
反応物LactideHCID 7272—
反応物1-DecanolHCID 8174—
反応物2-ethylhexanoic acid tin(II) saltHCID 9318—
反応物epsilon-CAPROLACTONEHCID 10401—
反応物GlycolideHCID 65432—
生成物PoliglecaproneHCID 65431—

反応条件

温度170 °C

反応手順

Glycolide (0.13 moles) was mixed with ε-caprolactone (1.18) and a catalytic amount of stannous octoate (0.262 mole) and 1-decanol (3.275 mole). The system was heated to 170° C. and was stirred at this temperature for 30 minutes. The reaction was then cooled to 120° C. Glycolide (0.65 moles) and dl-lactide (0.52 moles) were added to the prepolymer. After melting the second charge, the system was heated to 170° C. and was stirred at this temperature for 6.5 hours. At the conclusion of the reaction, the unreacted monomer was removed by heating at 130° C. under reduced pressure for 1.5 hours. The resulting polymer was characterized by DSC (for Tm), solution viscosity (for molecular dimensions), IR and NMR (for chemical composition).

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US06299631B1
出典データセットuspto-grants-2001_10
ORD IDord-1c558c26d9dd4b188c9a0b7c258b08d4
出典メモuspto-grants-2001_10