Styrene → Butyl prop-2-enoate;styrene

https://huagongshe.com/reaction/384583

反応式

関与物質

役割名称HCID仕込み量
反応物StyreneHCID 7501—
反応物Butyl AcrylateHCID 8846—
反応物Potassium PersulfateHCID 24412—
反応物PotassiumHCID 5462222—
溶媒WaterHCID 962—
生成物Butyl prop-2-enoate;styreneHCID 168422—

反応条件

温度60 °C

反応手順

In a 200-liter reactor equipped with a stirrer, a cooling apparatus, a condenser and a monomer supplying tube, 5 parts by weight of butylacrylate, 15 parts by weight of styrene, 0.2 parts by weight of triallyl isocyanurate, 140 parts by weight of ion-exchanged water and 1.0 parts by weight of potassium rosinate are added and mixed. The temperature is raised to 60° C. with stirring. After 10 minutes from the time of reaching 60° C., 0.25 parts by weight of potassium persulfate dissolved in deionized water is added thereto to initiate polymerization. The temperature of the reactor is maintained at 70° C. for 60 minutes. The polymerization is carried out at 70° C. for an additional 30 minutes to give an inner core of butylacrylate-styrene copolymer.

情報源と証拠

DOI10.6084/m9.figshare.5104873.v1
特許番号US08367770B2
出典データセットuspto-grants-2013_02
ORD IDord-6308c29c53df4acabed5aeb9c47e1454
出典メモuspto-grants-2013_02