関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Phosphoric Acid | HCID 1004 | — |
| 反応物 | Zirconium | HCID 23995 | — |
| 反応物 | Zirconium hydroxide (Zr(OH)4), (T-4)- | HCID 84465 | — |
| 反応物 | Phosphorus | HCID 5462309 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | Zirconium phosphate | HCID 160986 | — |
反応手順
Catalyst preparation. A zirconium phosphate based catalyst was prepared by a co-precipitation method. A solution of zirconium hydroxide (Zr(OH)4) as a zirconium precursor was dissolved in deionized water. To this solution, a stoichiometric amount of phosphoric acid as a phosphorus precursor was added. The resulting mixture was heated at 80° C. for 2 hours to remove water, and a paste was obtained. The resulting paste was then dried in an oven at 100° C. overnight (about 12-18 hours) to remove the bulk of any remaining water, and to provide a powder. The powder was then calcined at 350° C. for 2 hours to obtain powdered zirconium phosphate.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US08741258B2 |
|---|
| 出典データセット | uspto-grants-2014_06 |
|---|
| ORD ID | ord-5158bc0245e144c6ba10bfddbe185877 |
|---|
| 出典メモ | uspto-grants-2014_06 |
|---|