関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Phosphoric Acid | HCID 1004 | — |
| 反応物 | Phosphate | HCID 1061 | — |
| 反応物 | Zirconium | HCID 23995 | — |
| 生成物 | Zirconium phosphate | HCID 160986 | — |
反応手順
A zirconium phosphate film was prepared by adding a stoichometric amount of phosphate in the form of phosphoric acid to a solution of zirconium bound to PEI. The solution was then spin coated onto a glass slide and thermally treated at 1° C. to 120° C. with a dwell time of 30 minutes followed by heating to 350° C. at 1° C./minute with a dwell time of 30 minutes followed by heating to 450° C. at 1° C./minute with a dwell time of 1 hour and then cooling to 25° C.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US08530554B1 |
|---|
| 出典データセット | uspto-grants-2013_09 |
|---|
| ORD ID | ord-cf4b6531eeb34d11a932e26327e1f566 |
|---|
| 出典メモ | uspto-grants-2013_09 |
|---|