関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | tert-Butyl hydroperoxide | HCID 6410 | — |
| 反応物 | Styrene | HCID 7501 | — |
| 反応物 | Acrylonitrile | HCID 7855 | — |
| 反応物 | Ethylenediaminetetraacetic acid disodium salt | HCID 13020083 | — |
| 反応物 | Sodium Formaldehyde Sulfoxylate | HCID 23689980 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | Prop-2-enenitrile--ethenylbenzene (1/1) | HCID 62696 | — |
反応手順
After the solution temperature inside the reaction vessel decreased to 60° C., an aqueous solution having 0.4 parts of Rongalite dissolved in 10 parts of distilled water was added. Subsequently, a mixed solution including 11.1 parts of acrylonitrile, 33.2 parts of styrene, and 0.2 parts of tertiary butyl hydroperoxide was dropwise added thereto over about 1 hour to effect polymerization. After the completion of the dropwise addition, the resulting mixture was allowed to stand for 1 hour, and an aqueous solution having 0.0002 parts of ferrous sulfate, 0.0006 parts of disodium ethylenediaminetetraacetate, and 0.25 parts of Rongalite dissolved in 10 parts of distilled water was then added thereto. Subsequently, a mixed solution including 7.4 parts of acrylonitrile, 22.2 parts of styrene, and 0.1 parts of tertiary butyl hydroperoxide was dropwise added thereto over about 40 minutes to effect polymerization. After the completion of the dropwise addition, the resulting mixture was allowed to stand for 1 hour, and was then cooled down, thereby yielding a graft copolymer mixture latex in which an acrylonitrile-styrene copolymer was grafted onto the composite rubber composed of polyorganosiloxane and the butyl acrylate rubber.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US08536248B2 |
|---|
| 出典データセット | uspto-grants-2013_09 |
|---|
| ORD ID | ord-c2e837a084044280956adcd973545a67 |
|---|
| 出典メモ | uspto-grants-2013_09 |
|---|