Methane → Benzene, ethenyl-, polymer with 1,3-butadiene

HRID 466953
印刷

反応式

HRID 466953 の反応式
ClCl.CO.C.[CH3:6][CH2:7][CH2:8][CH2:9]CCCC[CH2:14][CH2:15][CH2:16][CH2:17][CH2:18][CH2:19][CH2:20][CH2:21][N+]1C=CC=CC=1.[Cl-]>C(Cl)(Cl)(Cl)Cl>[CH2:6]=[CH:7][CH:8]=[CH2:9].[CH2:21]=[CH:20][C:19]1[CH:14]=[CH:15][CH:16]=[CH:17][CH:18]=1
参加物実験手順後処理出典と根拠反応ノート

参加物

6

反応物 4

HCID 297MethaneHCID 887MethanolHCID 24526Chlorine2 回HCID 31239Cetylpyridinium Chloride

生成物 1

HCID 62697Benzene, ethenyl-, polymer with 1,3-butadiene

試薬・触媒・溶媒 1

HCID 5943Carbon Tetrachloride溶媒

実験手順

In an evacuated one liter beverage bottle equipped with a rubber septum and stir bar was added ten grams of polymer XVIII in carbon tetrachloride (100 grams). The solution was treated with 900 milliliters (0.04 mol, 2.6 grams) of chlorine gas introduced into the solution via cannula. After one hour, methanol (500 milliliters) was added to the reaction mixture to precipitate a white product. After filtration and vacuum drying, the resultant polymer had two glass transition temperatures at 52° and 72° C. as determined by DSC. The area under the 72° C. glass transition was approximately one-third the area under the 52° C. transition. When the same reaction was repeated using 450 milliliters of (0.02 mol, 1.3 grams) chlorine gas under the same conditions, a polymer product was obtained with a glass transition temperature at 50° C. The minimum fix temperature of this polymer as toner by extrusion with 6 weight percent of Regal® 330 carbon black and 2 percent of cetyl pyridinium chloride charge control agent was 240° F. and the hot offset temperature was 290° F. with a Xerox Corporation 5028™ silicone roll fuser operated at 3.3 inches per second.

後処理

  1. customIn an evacuated one liter beverage bottle equipped with a rubber septum
  2. additionintroduced into the solution via cannula
  3. customto precipitate a white product
  4. filtrationAfter filtration and vacuum
  5. customdrying
  6. customat 52°
  7. custom72° C.
  8. customunder the 72° C. glass transition
  9. customunder the 52° C. transition
  10. customWhen the same reaction
  11. customa polymer product was obtained with a glass transition temperature at 50° C
  12. customwas 240° F.

出典と根拠

ORDレコード
ord-94f998876fa140438010e4c6c6319e5f
出典データセット
uspto-grants-1992_10
DOI
10.6084/m9.figshare.5104873.v1
特許番号
US05158851

反応ノート