関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Isoprene | HCID 6557 | — |
| 反応物 | Styrene | HCID 7501 | — |
| 反応物 | 1,3-Butadiene | HCID 7845 | — |
| 溶媒 | Methanol | HCID 887 | — |
| 生成物 | Isoprene butadiene | HCID 168288 | — |
反応手順
Into a dried pressure vessel purged with nitrogen, 80 L of cyclohexane solvent and 0.34 L of sec-butyllithium initiator (10% by mass solution in cyclohexane) were charged. After raising the temperature to 50° C., 4.0 L of styrene was added to allow the polymerization to proceed for 3 h. Then, the polymerization was allowed to proceed for 4 h after adding a mixed liquid of 14.2 L of isoprene and 11.6 L of butadiene and further for 3 h after adding 4.0 L of styrene. The resultant reaction liquid was poured into 80 L of methanol, and the precipitated solid matter was separated by filtration and dried at 50° C. for 20 h, to obtain a polystyrene block-poly(isoprene/butadiene) block-polystyrene block, triblock copolymer.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US09102849B2 |
|---|
| 出典データセット | uspto-grants-2015_08 |
|---|
| ORD ID | ord-535c8e99255c4eebafa4032744d1ef33 |
|---|
| 出典メモ | uspto-grants-2015_08 |
|---|