関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Urethane acrylate | HCID 21863578 | — |
| 反応物 | Dipentaerythritol caprolactone | HCID 66608674 | — |
| 反応物 | Pentaerythritol hexaacrylate | HCID 131731916 | — |
| 溶媒 | Isopropanol | HCID 3776 | — |
| 生成物 | 1-Hydroxycyclohexyl phenyl ketone | HCID 70355 | — |
反応手順
A protective layer coating solution was prepared by mixing 3 parts by mass of pentaerythritol hexaacrylate (KAYARAD DPHA, produced by Nippon Kayaku Co., Ltd.), 3 parts by mass of an urethane acrylate oligomer (ART RESIN UN-3320HA, produced by Negami Chemical Industrial Co., Ltd.), 3 parts by mass of an acrylic acid ester of dipentaerythritol caprolactone (KAYARAD DPCA-120, produced by Nippon Kayaku Co., Ltd.), 1 part by mass of a silica (P-526, produced by Mizusawa Industrial Chemicals, Ltd.), 0.5 parts by mass of a photopolymerization initiator (IRGACURE 184, produced by Nihon Ciba-Geigy K.K.), and 11 parts by mass of isopropyl alcohol, and sufficiently agitating and dispersing the mixture with the use of a ball mill, such that the average particle diameter became approximately 3 μm.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US08852856B2 |
|---|
| 出典データセット | uspto-grants-2014_10 |
|---|
| ORD ID | ord-8b9d069eb1fd492a9b508b48fd643f04 |
|---|
| 出典メモ | uspto-grants-2014_10 |
|---|