関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Acrylamide | HCID 6579 | — |
| 反応物 | Potassium Persulfate | HCID 24412 | — |
| 反応物 | 2-Propenamide, N-octyl- | HCID 82370 | — |
| 反応物 | Sodium vinylsulfonate | HCID 3270262 | — |
| 反応物 | Sodium Lauryl Sulfate | HCID 3423265 | — |
| 溶媒 | Methanol | HCID 887 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | N-Octylacrylamide Acrylamide Vinyl Sulfonate | HCID 86742029 | — |
反応手順
A one liter Morton style resin kettle, fitted with a chilled water condenser, thermometer, nitrogen sparger and mechanical stirrer was charged with 500 ml of purified water. The water was refluxed for 1 hour with a nitrogen purge and then cooled to room temperature. Acrylamide, 9.886 g (0.14 mole), 4.81 g (0.37 mole) of sodium vinyl sulfonate as a 25% solution in water, 0.33 g (0.002 mole) of N-octylacrylamide and 15 g of sodium dodecyl sulfate (SDS) were charged into the flask. The reaction solution was heated to 50° C. and 0.01 g potassium persulfate was added. After 17 hours at 50° C. and 300 rpm stirring, the viscous solution was slowly poured into 3 L of methanol and the precipitated polymer was isolated by filtration. The polymer was then masticated in a Waring blender with 2 L of methanol for 30 seconds, filtered and dried under vacuum at room temperature. The yield of the polymer was 10.9 g.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US04730028 |
|---|
| 出典データセット | uspto-grants-1988_03 |
|---|
| ORD ID | ord-bd2c09e4fa2941e1be28610657c18648 |
|---|
| 出典メモ | uspto-grants-1988_03 |
|---|