関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Acrylamide | HCID 6579 | — |
| 反応物 | 2-Propenamide, N-octyl- | HCID 82370 | — |
| 反応物 | Sodium styrenesulfonate | HCID 53627496 | — |
| 溶媒 | Methanol | HCID 887 | — |
| 生成物 | N-Octylacrylamide Acrylamide Sodium Styrene Sulfonate | HCID 86742030 | — |
反応手順
A solution of 15.0 g of SDS in 500 ml of purified, deoxygenated water was prepared and 0.415 g of N-octylacrylamide, 12.73 g of acrylamide and 9.35 g of sodium styrene sulfonate were added. The resulting clear solution was placed in a 2 liter Morton style resin kettle fitted with a chilled water condenser, thermometer, nitrogen sparger and mechanical stirrer. The solution was purged with nitrogen for 0.5 hour at 25° C., then 0.116 g of potassium persulfate and 0.0082 g of sodium metabisulfite were added. After 16 hours of stirring at 300 rpm and 25° C. the reaction mixture was slowly poured into 3 L of acetone. The precipitated polymer was isolated and masticated with 1 L of methanol in a Waring blender for 30 seconds, filtered and dried under vacuum at 30° C. The yield of polymer was 5.14 g.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US04730028 |
|---|
| 出典データセット | uspto-grants-1988_03 |
|---|
| ORD ID | ord-1f131f8a52a5430b8710219ac2ce5ea1 |
|---|
| 出典メモ | uspto-grants-1988_03 |
|---|