[C:1]([O-:20])(=[O:19])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13]CCCCC.[Al+3].[C:22]([O-])(=[O:40])[CH2:23]CCCCCCCCCCCCCCCC.C([O-])(=[O:60])CCCCCCCCCCCCCCCCC.C([O-])(=O)CCCCCCCCCCCCCCCCC.[Li+]>>[C:13]1(=[O:60])[O:40][CH2:22][CH2:23][O:20][C:1](=[O:19])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12]1参加物
3
反応条件
- 温度
- 314 °C
実験手順
A mixed metal catalyst comprised of aluminum stearate and lithium stearate (molar ratio 1:1) was used for the depolymerization. For the reaction aluminum stearate (1.09 gram) and lithium stearate (0.36 gram) were blended in 70 grams poly(ethylene brassylate) at 200° C. The temperature was then raised to 314° C. while maintaining a vacuum of 0.05-0.1 mm Hg. Ethylene brassylate was obtained (40 mls during the first hour) in an 88.9 percent yield. Of the ethylene brassylate recovered, 90 percent of the product was obtained after 2 hours.
後処理
- temperaturewhile maintaining a vacuum of 0.05-0.1 mm Hg
出典と根拠
- ORDレコード
- ord-0f676f5a41704569b949cc4c945350ba
- 出典データセット
- uspto-grants-1985_02
- 特許番号
- US04499288
関連ノート
読み込み中…