関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Sodium Carbonate | HCID 10340 | — |
| 反応物 | Ammonium Chloride | HCID 25517 | — |
| 反応物 | Neodymium(3+) trichloride | HCID 10131187 | — |
| 触媒 | Cobalt(II) chloride | HCID 24288 | — |
| 生成物 | Neodymium sesquicarbonate | HCID 167103 | — |
反応手順
A solution of cobalt chloride having a gravity of 1.20 g/cm3 containing ammonium chloride was mixed while stirring with a solution of neodymium chloride and heated to 50° C. A stoichiometric equivalent quantity of sodium carbonate solution of 60° C. having a gravity of 1.05 g/cm3 was added to the mixed solution while stirring. The precipitates of cobalt carbonate and neodymium carbonate were obtained after reaction, filtrated in a vacuum filtrator to remove the mother liquid, washed by distilled water of 90° C. for 6 times, dried at 200° C., crushed and sieved by a 20 mesh sieve, reduced at 600° C. in hydrogen for 3 h, then crushed again and sieved by a 100 mesh sieve. The prepared cobalt powder contained 2.8% (wt.) neodymium.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US05248328 |
|---|
| 出典データセット | uspto-grants-1993_09 |
|---|
| ORD ID | ord-155ed44d0c004f6b88a366ddb1f96444 |
|---|
| 出典メモ | uspto-grants-1993_09 |
|---|