反応式
[C:1]([C:5]1[CH2:10][C:9](C(C)(C)C)(C)[CH:8]=[CH:7][C:6]=1O)(C)(C)[CH3:2]>C1(C)C=CC=CC=1.C(O)(C)C>[CH2:2]=[CH:1][C:5]1[CH:10]=[CH:9][CH:8]=[CH:7][CH:6]=1.[CH2:2]=[CH:1][CH:5]=[CH2:6].[CH2:2]=[CH:1][C:5]1[CH:10]=[CH:9][CH:8]=[CH:7][CH:6]=1参加物
3
実験手順
Following the completion of Step III, 2,4-di-t-butyl-4-methylphenol (one part by weight per hundred parts of total monomers) was added as a 10 weight percent solution in 50/50 (by volume) toluene/isopropyl alcohol, and the polymer recovered by adding the polymerization mixture to isopropyl alcohol. The coagulated polymer was collected by filtration and dried under reduced pressure. Physical properties of the butadiene/styrene teleblock polymer prepared by this procedure are shown in Table I.
後処理
- customthe polymer recovered
- additionby adding the polymerization mixture to isopropyl alcohol
- filtrationThe coagulated polymer was collected by filtration
- customdried under reduced pressure
- customPhysical properties of the butadiene/styrene teleblock polymer prepared by this procedure
出典と根拠
- ORDレコード
- ord-a2e23f37504149c3bd39beb3611b2db2
- 出典データセット
- uspto-grants-1978_12
- 特許番号
- US04131725
関連ノート