関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Acrylic Acid | HCID 6581 | — |
| 反応物 | Sodium Hydroxide | HCID 14798 | — |
| 反応物 | Sodium Persulfate | HCID 62655 | — |
| 反応物 | alpha-Methylene butyrolactone | HCID 68352 | — |
| 反応物 | Allyl pentaerythritol | HCID 3086330 | — |
| 反応物 | Sodium Lauryl Sulfate | HCID 3423265 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | alpha-Methylene-gamma-butyrolactone acrylic acid pentaerythritol allyl ether | HCID 131731900 | — |
反応手順
The crosslinked polymer poly(α-methylene-γ-butyrolactone-acrylic acid-pentaerythritol allyl ether) was prepared by emulsion polymerization of α-methylene-γ-butyrolactone and acrylic acid with the crosslinking monomer pentaerythritol allyl ether. To a four neck round bottom glass flask, equipped with a mechanical stirrer and a thermocouple with a nitrogen inlet at the side of the inlet-tube and two dropping funnels was added the initial charge of 44.03 g of water and 0.51 g of a 20% solution of sodium dodecyl sulfate surfactant. Into the monomer dropping funnel a mixture of 20.8 g of α-methylene-γ-butyrolactone, 1.1 g of acrylic acid and 0.16 g of pentaerythritol allyl ether were added. Into the second dropping funnel the aqueous mixture consisting of 83.43 g water, 1.32 g 20% sodium dodecylsulfate, 0.14 g sodium persulfate and 0.17 g 20% sodium hydroxide solution were added. The initial charge was heated to 75° C. dropwise addition of the monomer was started. Dropwise addition of the aqueous mixture started 5 minutes later. The monomer feed ended 120 minutes after the start of monomer addition, and the aqueous stream ended 5 minutes after the monomer stream ended. After a cook-down time of one hour, the reaction mixture was cooled to room temperature.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US08846817B2 |
|---|
| 出典データセット | uspto-grants-2014_09 |
|---|
| ORD ID | ord-40aa735a4fc642b2855ba315df9fa102 |
|---|
| 出典メモ | uspto-grants-2014_09 |
|---|