反応式
[CH:1]1[CH:2]=[CH:3][N+:4]([O-:8])=[C:5]([SH:7])[CH:6]=1.S([O-])([O-])(=O)=O.[Zn+2:14].[Cl-].[Zn+2].[Cl-].C([O-])(=O)C.[Zn+2].C([O-])(=O)C>O>[CH:1]1[CH:2]=[CH:3][N:4]([O-:8])[C:5](=[S:7])[CH:6]=1.[CH:1]1[CH:2]=[CH:3][N:4]([O-:8])[C:5](=[S:7])[CH:6]=1.[Zn+2:14]参加物
6
実験手順
In another aspect, the present invention relates to a method for producing submicron-sized particles of zinc pyrithione comprising reacting a pyrithione or a water-soluble salt of pyrithione and a water-soluble zinc salt selected from the group consisting of zinc sulfate, zinc chloride, zinc acetate, and combinations thereof, in a turbulent flow reactor generating pulverizing forces, the turbulent flow reactor maintained at a pressure of from about 18,000 psi to about 23,000 psi and a temperature of from about 0° C. to about 23° C., the reaction producing submicron-sized particles of zinc pyrithione.
後処理
- customin a turbulent flow reactor generating pulverizing
- temperatureforces, the turbulent flow reactor maintained at a pressure of from about 18,000 psi to about 23,000 psi
出典と根拠
- ORDレコード
- ord-483c0a762d304aa9bcdefbcf02986870
- 出典データセット
- uspto-grants-2000_01
- 特許番号
- US06017936
関連ノート
読み込み中…