関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Adipic Acid | HCID 196 | — |
| 反応物 | Trimethylolpropane | HCID 6510 | — |
| 反応物 | Acrylic Acid | HCID 6581 | — |
| 反応物 | 2-ethylhexanoic acid tin(II) salt | HCID 9318 | — |
| 反応物 | 2,6-Di-tert-butyl-4-methylphenol | HCID 31404 | — |
| 反応物 | Hexanediol | HCID 147023 | — |
| 反応物 | Diisocyanatotoluene | HCID 12905475 | — |
| 反応物 | Isophorone DI-isocyanate | HCID 21298402 | — |
| 生成物 | Urethane acrylate | HCID 21863578 | — |
反応手順
661.9 g of the ethylene oxide polyether started from trimethylolpropane esterified with 2 mol acrylic acid (12 mol ethylene oxide per mol trimethylolpropane) and 164.4 g of a polyester polyol from hexanediol and adipic acid (OH number 314, equivalent weight 178.5 g), 1.0 g 2,6-di-tert-butyl-4-methyl-phenol and 1.0 g tin octoate were initially introduced into the reaction vessel. 148.8 g Desmodur® T80 (toluylene diisocyanate, commercial product of Bayer AG, Leverkusen) were metered in at 50 to 60° C. After a further 5 h 31.6 g isophorone-diisocyanate were metered in. The reaction was carried out at 60° C. for a further 5 h and 74.0 g of the ethylene oxide polyether started from trimethylolpropane esterified with 2 mol acrylic acid (12 mol ethylene oxide per mol trimethylolpropane) were then added. The reaction was subsequently carried out at 60° C. until the NCO content of the solution was less than 0.10 wt. %.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US06465539B1 |
|---|
| 出典データセット | uspto-grants-2002_10 |
|---|
| ORD ID | ord-a94cf400ad4f479eaaee61752ae937bd |
|---|
| 出典メモ | uspto-grants-2002_10 |
|---|