Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Phosphoric Acid → Phosphate cerium nitrate
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Phosphoric Acid | HCID 1004 | — |
| 반응물 | Cerium nitrate | HCID 24948 | — |
| 반응물 | Bentone | HCID 56841936 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | Phosphate cerium nitrate | HCID 86755301 | — |
반응 단계
A clay/phosphate/cerium nitrate solution was prepared (according to the general teachings of U.S. Pat. No. 5,190,902) by adding 1403 grams of Theile RC-32® kaolin clay slurry to 591 milliliters of water in a high speed mixer. To this mixture, 192 grams of phosphoric acid was then added. To the resulting system, 440 grams of cerium nitrate solution was added. The slurry formulation was then spray dried and the resulting particles calcined at 650° C. for 30 minutes in a muffle furnace. The calcined particles were then mixed with magnesium oxide in a 50/50 weight percent ratio and the resulting material analyzed by a TGA test that showed a SOx absorption rate of 0.21% per minute for the end product material.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US06048821 |
| 출처 데이터셋 | uspto-grants-2000_04 |
| ORD ID | ord-747e4b03de5847b084505250e771a301 |
| 출처 메모 | uspto-grants-2000_04 |